MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott RayVolution® D99 Sodium-Potassium-Barium-Silicate Glass
Categories: Ceramic; Glass; Optical

Material Notes: Highly UV-transmitting. Used as envelope for germicidal lamps (low pressure mercury vapor discharge lamps) and for UV detectors.

The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppm

Information provided by SCHOTT AG.

Vendors: SCHOTT with its Business Unit Tubing offers tailor-made products & services worldwide from more than sixty special glass types for international growth markets such as industrial and environmental technology, electronics, display industry, architecture and design as well as pharmaceuticals. Contact us.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.52 g/cc
@Temperature 25.0 °C
0.0910 lb/in³
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.90 µm/m-°C
@Temperature 20.0 - 300 °C
5.50 µin/in-°F
@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 480 °C896 °FISO 7884-8
Softening Point 675 °C1250 °FViscosity 107.6 dPa s; ISO 7884-3
Working Point 995 °C1820 °FViscosity 104 dPa s; ISO 7884-2
Annealing Point 490 °C914 °FViscosity 1013 dPa s; ISO 7884-4
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.506
@Wavelength 587.6 nm
1.506
@Wavelength 587.6 nm
UV Transmittance >= 75 %
@Thickness 1.00 mm,
Wavelength 254 nm
>= 75 %
@Thickness 0.0394 in,
Wavelength 254 nm
 
Descriptive Properties
Acid ResistanceClass S2DIN 12116
Alkali ResistanceClass A3ISO 695
Hydrolytic ResistanceClass HGB 5ISO 719

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSGS948 / 291336

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.