MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rogers Arlon Flexible Silicon Insulation with Fiberglass Substrate (56493F031)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Silicone

Material Notes: Side one - cured silicone rubber ,0.007 in. (0.18 mm) minimum: Substrate - Prime Coated 1564 Fiberglass, 0.017 in. (0.43 mm) nominal; Side two- cured silicone rubber, 0.007 in. (0.18 mm) minimum; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.031 in ±0.0025 (0.79 mm ± 0.063). Color: Blue-black. Weight: 1122 g/m² ± 102 (33.1 oz./yd.² ± 3.0). Shelf Life: 12 months from the date of manufacture. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Flame Test Method: FTMS 191A; Method 5903. Maximum Flame and Glow Time: 25 seconds. Maximum Char Length: 7.62 cm (3 in).

Information provided by the manufacturer, Arlon Silicone Technologies Division.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 45 - 5545 - 55
Tensile Strength, Ultimate 7.61 - 8.99 MPa1100 - 1300 psi
Elongation at Break 300 - 500 %300 - 500 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.75 kV/mm>= 400.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -97.8 °C-144 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb
Titanium Carbide, TiC
Vicone High Performance Rubber VicoSil™ 139DLK-BL High Performance Silicone Rubber
BIW Silicone Rubber Extrusions, Standard Grades
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles

PASE20 / 24741

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.