WN503AE is a 50 % mineral filled high performance masterbatch. It is typically used in combination with RTPO base polymers and blended directly on the injection molding machine in order to achieve the desired material mechanical property profile. Applications: WN503AE has been developed especially for the car industry to be used in automotive exterior parts. - Bumpers
- Exterior trims
- Automotive exterior applications
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.Information provided by Borealis AG |