MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an excellent soft touch feel, will bond to olefinics, is easy to color, and is available in FDA compliant formulations. DuraGrip® is not hygroscopic and under normal conditions does not require drying.

Information provided by Advanced Polymer Alloys

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccASTM D471; ISO 2781
Viscosity 107000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
ASTM D3835
Linear Mold Shrinkage 0.013 cm/cm
 0.022 cm/cm
Linear Mold Shrinkage, Transverse 0.010 cm/cm
 0.015 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63Time of 5 seconds; ASTM D2240; ISO 48
Tensile Strength, Ultimate 946.88 psiAfter 7 days at 70°C; ASTM D412 ISO 37
 1001 psiAfter 7 days at 100°C; ASTM D412 ISO 37
 1076 psiASTM D412; ISO 37
Elongation at Break 370.44 %After 7 days at 70°C; ASTM D412 ISO 37
 378 %ASTM D412; ISO 37
 378 %After 7 days at 100°C; ASTM D412 ISO 37
Modulus of Elasticity 0.314 ksiAfter 7 days at 70°C; ASTM D412 ISO 37
 0.334 ksiAfter 7 days at 100°C; ASTM D412 ISO 37
100% Modulus 0.318 ksi
@Strain 100 %
ASTM D412; ISO 37
Graves Tear Strength 132 pli
@Temperature 23.9 °C
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 30Cs-17 Wheel, 1000 g Load; ASTM D3389
Compression Set 43 %
@Temperature 70.0 °C
22 hrs.; ASTM D395; ISO 815
 71 %
@Temperature 100 °C
22 hrs.; ASTM D395; ISO 815
 23 %
@Temperature 24.0 °C,
Time 79200 sec
ASTM D395; ISO 815
Tensile Set 11 %100% Tension; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -89.0 °FASTM D746; ISO 812
 
Processing PropertiesOriginal ValueComments
Processing Temperature 400 °F
Rear Barrel Temperature 370 - 390 °F
Middle Barrel Temperature 390 - 410 °F
Front Barrel Temperature 420 - 440 °F
Nozzle Temperature 400 - 430 °F
Melt Temperature 390 - 430 °F
Mold Temperature 110 - 130 °F
Injection Pressure 150 - 500 psi
Cycle Time - Injection 0.50 - 2.0 secboost
Screw Speed 25 - 100 rpm
Cure Time 10.0 - 20.0 secCooling Time
 
Descriptive Properties
Fluid Resistance - Volume Change, % (ASTM D471)-13After 7 Days in Water at 212°F (100°C)
 2After 7 Days in ASTM Oil No.1 at 212°F (100°C)
 39After 7 Days in IRM 903 Oil No.3 at 212°F (100°C)
 9After 7 Days in ASTM Ref. Fuel No. B at 75°F (24°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer
6060 Aluminum Composition Spec
A. Schulman Alcryn® 2170 BK Melt Processable Rubber
A. Schulman Alcryn® 2160 BK Melt Processable Rubber
A. Schulman Alcryn® 1060 BK Melt Processable Rubber

PAPA036 / 24103

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.