MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Categories: Metal; Metal Foam, Mesh, or Honeycomb; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the face sheets that carry bending loads and the honeycomb that carries the shear loads. The adhesive is the interface between the facing and the core in the same way that the oxide on the aluminum and the primer that has been applied to it is the interface between the honeycomb substrate material and the bonding adhesive. This interface is critical to the performance of honeycomb bonded assemblies.

HexWeb® CR-PAA™ is designed for aircraft structures that are exposed to demanding environmental conditions. HexWeb® CR-PAA™ outperforms standard MIL-C-7438 core in salt spray and HexWeb® crack propagation tests.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0721 g/cc0.00260 lb/in³Nominal
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength >= 2.59 MPa>= 375 psiBare, min
 >= 2.79 MPa>= 405 psiStabilized, min
 3.79 MPa550 psiBare, typical
 3.93 MPa570 psiStabilized, typical
Compressive Modulus 1.03 GPa150 ksiStabilized, typical
Shear Modulus 0.214 GPa31.0 ksiPlate Shear, W Direction, typical
 0.483 GPa70.0 ksiPlate Shear, L Direction, typical
Shear Strength >= 1.16 MPa>= 168 psiPlate Shear, W Direction, min
 1.52 MPa220 psiPlate Shear, W Direction, typical
 >= 1.97 MPa>= 285 psiPlate Shear, L Direction, min
 2.34 MPa340 psiPlate Shear, L Direction, typical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum, Al
Borosilicate Glass
Solvay Chemicals PHOSPHORIC ACID 80% - 87%
Hexcel® HexWeb® CR III 1/4-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb

PHEXC269 / 98740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.