MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ LUBRICOMP™ Compound LX91475 Polyetheretherketone (PEEK) (Asia)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP LUBRICOMP LX91475 compound is based on Polyetheretherketone (PEEK) resin containing proprietary fillers. Added features of this grade include: Easy Molding, High Temperature Bearing Grade, Wear Resistant.

Features: Bearing Grade,Good dimensional stability,Wear resistant,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 139 MPa20200 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Tensile Modulus 11.03 GPa1600 ksi50 mm/min; ASTM D638
Flexural Strength 206 MPa29900 psiASTM D790
Flexural Modulus 10.34 GPa1500 ksiASTM D790
Izod Impact Notched 58.0 J42.8 ft-lbASTM D256
Izod Impact, Unnotched 4.80 J/cm8.99 ft-lb/inASTM D4812
Coefficient of Friction, Dynamic 0.350.35ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.230.23ASTM D3702 Modified: Manual
K (wear) Factor 24.2 x 10-8 mm³/N-M12.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
@Thickness 3.20 mm
554 °F
@Thickness 0.126 in
unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80890 / 288837

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.