MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Aremco-Bond™ 525-N Electrically & Thermally Conductive Epoxy, Silver Filled
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Silver-Filled, Electrically & Thermally Conductive, Heat Cured, One-Part Epoxy Paste to 340°F.

Vendors: Aremco offers a broad line of electrically and thermally conductive adhesives and greases for applications from room temperature to 1700°F (927°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.85 g/cc
@Temperature 25.0 °C
mixed
Particle Size <= 28 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76
Shear Strength 2500 psiASTM D1002-94
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.006 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.10 W/m-K
Maximum Service Temperature, Air 340 °Fcontinuous
 375 °Fintermittent
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 149 °C
Recommended Cure
 6.00 hour
@Temperature 121 °C
Alternative Cure
Shelf Life 6.00 Month
 
Descriptive Properties
ColorSilver
FillerSilver Flake
Mixed ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAREM16w / 256043

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.