MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt DISTITRON® 114 C Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, DCPD

Appearance: Yellow - Transparent

Main resin characteristics: Low styrene content, Clear, unaccelerated

Main applications: Flat sheets, laminates

Molding information: Continuous laminating

Curing cycle: 24h at 23°C + 2h at 100°C + 1h at 100°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
Solids Content 65 - 69 %MT-CU001C
Brookfield Viscosity 260 - 340 cPsp 2 rpm 20; MT-CUT23V
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 40ASTM D 2583
Tensile Strength 70.0 MPaISO 527
Elongation at Break 2.5 %ISO 527
Tensile Modulus 3600 MPaISO 527
Flexural Strength 130 MPaISO 178
Flexural Modulus 3500 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CISO 75 -2A
Glass Transition Temp, Tg 98.0 °CASTM E 1545
 
Processing PropertiesOriginal ValueComments
Gel Time 13.0 - 16.0 min
@Temperature 25.0 °C
Reactivity at 25°C + 0,2% Co 6% + 1,5% Perox; RS.08.G
Shelf Life 4.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm175 - 205°CRS.08.G; Reactivity at 25°C + 0,2% Co 6% + 1,5% Perox

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9376 / 231971

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.