MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical 1.3-Butadiene
Categories: Fluid

Material Notes: Physical Properties: Colorless, Slightly Sweet taste, Narcotic gas, Easy polymerization and addition reaction

Structure & Characteristics: CH2=CH-CH=CH2. Unsaturated fatty acid hydrocarbon. Has a characteristic odor in room temperature, and is an inflammable gas vaporized at -4.4°C. It readily vaporizes at 2~3 atm near 20°C

Uses: Shock absorber - by blending in Natural rubber, Tire, Shoes, Foam rubber, Paper coating, Electric appliance cases, Interior parts of automobile, Interior parts of automobile, Material for PBT resin, Adipic acid, Chloro Benzene Rubber.

CAS: 106-99-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.00188 g/ccgas
 0.620 g/ccliquid
Vapor Pressure 1810 torr
@Temperature 15.0 °C
Vapor Density=1.9
 
Thermal PropertiesOriginal ValueComments
Melting Point -144 °C
Boiling Point -4.40 °C
Flash Point -76.0 °C
Ignition Temperature 429 °CAutoignition
 
Descriptive Properties
Components1.2-BD<50 ppm
 1.3-BD>99%
 CARBONYLS<30 ppm
 DIMETHYL ACETYLENE<50 ppm
 NON VOLATILE MATTER<0.1 %
 PEROXIDES<10 ppm
 SOLVENT<10 ppm
 SULFUR<10 ppm
 TOTAL a ACETYLENE<60 ppm
 TOTAL ALLENE<50 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kapton® 100EN Polyimide Film, 25 Micron Thickness
Vanadium, V; Cold Rolled
Momentive Performance Materials Addisil™ 1070 E Industrial Extrusion Heat Cured Rubber
KKPC KOSYN KSL 341 Styrene-Butadiene Latex
Eurofoam Porocell POR 303/B CR-Neoprene/NBR Foam

PLAY774 / 148784

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.