MDI composition developed as isocyanate component of high resilience foams used in the automotive industry for sound insulation Uses: Flexible foams: High resilience polyurethane foams (HR), Automotive sound insulation Information provided by BorsodChem Rt. |
Methyl Diphenyl Diisocyanate |