MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Powerflow™ HE Hydraulic Oil ISO Grade 22
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Powerflow HE Hydraulic Oil is a premium quality, high viscosity index antiwear hydraulic oil developed for use in industrial and mobile equipment operating in cold climates or in locations subject to wide variations in ambient temperatures. It meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high-pressure, high-speed hydraulic pumps. It is particularly recommended for year-round use in mobile equipment such as bucket trucks, cranes and aerial lifts. Powerflow HE Hydraulic Oil is specially formulated to have a high viscosity index and a low pour point for use over a wider temperature range than conventional antiwear hydraulic oils. Its high viscosity index helps maintain oil viscosity at operating temperatures and reduce energy (power) loss caused by internal oil leakage in the hydraulic system, resulting in up to 6% higher system efficiency compared to conventional single-grade hydraulic oils. Powerflow HE provides excellent wear protection for hydraulic pumps and motors, has excellent oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life, and protects hydraulic system components against rust and corrosion. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foam buildup that can cause poor or sluggish hydraulic system response. It has excellent low-temperature properties for cold start-ups. It also has a high dielectric strength for use as insulating oil in electrical service bucket trucks.

Applications:

  • Industrial and mobile equipment operating in cold weather or in locations subject to wide temperature fluctuations
  • Bucket trucks (cherry pickers) used for servicing electrical power lines or for tree-trimming
  • Hydraulic hoists and service station lifts
  • Marine cargo winches and steering systems
  • Off-road construction, mining and marine equipment
  • Chain drives
  • Electric motor bearings Powerflow HE Hydraulic Oil meets the requirements of the following industry and OEM specifications:
    • DIN 51524 Part 3, Antiwear Hydraulic Oils, Type HVLP
    • Eaton-Vickers M-2950-S, I-286-S
    • ISO 11158:1997, Family H (Hydraulic Systems), Type HV
    • Parker Hannifin (Denison) HF-0, HF-1, HF-2
    Features/Benefits:
    • High VI to reduce internal oil leakage and increase hydraulic system efficiency by up to 6% compared to conventional single-grade hydraulic fluids
    • Excellent service over a wide temperature range
    • Excellent wear protection for hydraulic pumps and motors
    • Excellent oxidation resistance and thermal stability
    • High shear stability
    • Protects against rust and corrosion
    • Excellent water-separating properties
    • Good foam resistance
    • Excellent low-temperature properties for cold start-ups
    • High dielectric strength for use in electrical service bucket trucks (cherry pickers)

    Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.863 g/cc0.863 g/cc
Density 0.860 g/cc0.0311 lb/in³
Viscosity Measurement 173173Index
Saybolt Viscosity at 100°F 163 SUS163 SUS
Saybolt Viscosity at 210°F 48.6 SUS48.6 SUS
Kinematic Viscosity at 40°C (104°F) 32 cSt32 cSt
Kinematic Viscosity at 100°C (212°F) 6.7 cSt6.7 cSt
Oxidative Stability >= 5.0 hour>= 5.0 hourRPVOT; ASTM D2272
 >= 7000 hour>= 7000 hourTOST; ASTM D943-04a
ASTM Color 0.500.50ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.600.60[mg KOH/g]; ASTM D974
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.0 kV/mm889 kV/inASTM D877
 
Thermal PropertiesMetricEnglishComments
Pour Point -51.0 °C-59.8 °F
Flash Point 204 °C399 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn 0.066 %0.066 %
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility10 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5401 / 198654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.