MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Durostone® EPR S1 Epoxy Components
Categories: Polymer; Thermoset; Epoxy

Material Notes: Durostone® EPR S1 threaded rods consist of two main components, a special designed glass reinforcement and an embedding epoxy resin matrix. Durostone® EPR S1 is our standard grade for threaded rods and is successfully used for decades in many different areas.
  • Standard length: 1900 mm
  • Standard size: M8-M30
  • Threads in accordance with ISO 965
  • Tolerance zone 6g. all sizes in mm
Larger sizes on request

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ISO 1183 meth 1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 400 MPa58000 psiParallel; ASTM D5083
Modulus of Elasticity 20.0 GPa2900 ksiPerpendicular; ISO 178
Flexural Strength 500 MPa72500 psiPerpendicular; ISO 178
Compressive Strength 300 MPa43500 psiPerpendicular; ASTM D695
Charpy Impact, Notched 10.0 J/cm²47.6 ft-lb/in²Parallel; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 48.0 - 62.0 Hz
5.0
@Frequency 48.0 - 62.0 Hz
IEC 60250
Dielectric Strength 13.0 kV/mm
@Temperature 90.0 °C
330 kV/in
@Temperature 194 °F
Parallel; IEC 60243-1
Comparative Tracking Index 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 20.0 µm/m-°C5.56 - 11.1 µin/in-°F
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FISO 8302
Maximum Service Temperature, Air 180 °C356 °FThermal Endurance; IEC 60216
 
Descriptive Properties
Delamination load4000 NDIN 53463
Insulating classHIEC 60085

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9103 / 232806

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.