MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solvay MACKANATE® OPV Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Product Description: Mackanate® OPV is a vegetable derived sulfosuccinate half ester of oleamide MIPA. As such, it is a very mild surfactant to both eye and skin. When blended with high foaming anionic surfactants, like alpha olefin sulfonates, lauryl and laureth sulfates, Mackanate® OPV will reduce irritation without significantly reducing foam. Mackanate® OPV also responds readily to viscosity builders, such as, amides, betaines and salts. High viscosity products can be easily formulated. This grade is preserved with methylparaben, propylparaben and has no formaldehyde donors.

INCI Name: Disodium Oleamido MIPA Sulfosuccinate

CAS: 43154-85-4

EINECS: 256-120-0

Infrared Spectrum: Matches Spectrum

Uses: Mild Shampoos, Baby Shampoos, Bubble Baths, Bath Products and Body Cleansers

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³
Solids Content 36.5 - 39.5 %36.5 - 39.5 %Moisture Balance
pH 5.0 - 7.05.0 - 7.05% Solution
Viscosity <= 2000 cP<= 2000 cP#3 SP @ 12 rpm
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 6.0<= 6.0
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceClear Liquid
CompositionPathogenic OrganismsAbsent
 Total Plate Count<100 cfu/g
PreservativeMethyl Paraben0.001
 Propyl Paraben0.0002

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MACKANATE® OPV-N Surfactant
Verdant Specialty Solutions MACKAM® 2CSF-40CG Surfactant
Solvay MACKAM® 2CYSF Surfactant
Verdant Specialty Solutions MACKAM® 50-SB Surfactant
Solvay MACKADET® EQ-178 Surfactant

WRHOD220 / 137451

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.