Notes: Medalist MD-12100H Series are high performance thermoplastic elastomer designed for use in healthcare and medical applications requiring high flow. Medalist MD-12140H is a low hardness, low density, RoHS compliant, sterilizable grade suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Colorability; Good Flexibility; Good Moldability; Good Sterilizable; Good Toughness; Halogen Free; Low Density; High Flow; Low Hardness; Low Specific Gravity; Radiation (Gamma) Resistant; Resilient; Slip; Without Fillers Uses: Bladders; Bushings; Connectors; Disposable Hospital Goods; Flexible Grips; Grommets; Handles; Knobs; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement; Seals Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |