MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nordel® IP 4570 EPDM Hydrocarbon Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Nordel® IP 4570 is an amorphous EPDM grade designed for extruded applications. It is ideally suited for dense extruded profiles, coolant hose and general purpose moldings. The combination of high viscosity and low crystallinity allows for good balance of processability, extensibility, low-temperature properties and performance.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.860 g/ccASTM D297
Volatiles <= 0.40 %Total Volatiles; DuPont Dow PQ-E-007
Mooney Viscosity 70
@Temperature 125 °C
ML 1 + 4; ASTM D1646
Ash <= 0.10 %ASTM D5667
 
Descriptive Properties
ENB5 mass%ASTM D6047
Ethylene50 mass%ASTM D3900
Molecular Weight DistributionMediumDuPont Dow PQ-E-034 and 036
Product FormBale
Propylene45 mass%ASTM D3900
Residual Transition MetalMax 10 ppmDuPont Dow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nordel® IP 4640 EPDM Hydrocarbon Rubber
Dow Nordel® IP 4770P EPDM Hydrocarbon Rubber
Dow Nordel® IP 3670 EPDM Hydrocarbon Rubber
Dow Nordel® IP 4520 EPDM Hydrocarbon Rubber
Ethylene Propylene Rubber (EPM, EPDM)

PDVG13 / 34133

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.