MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Material Notes:

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 - 0.800 g/cc
Density 1.50 g/ccISO 1183
Water Absorption 1.6 %ISO 62
Moisture Absorption at Equilibrium 0.60 %23°C; 50% RH; ISO 62
Viscosity Test 56 cm³/gISO 307
Linear Mold Shrinkage, Flow 0.0036 cm/cmISO 2577, 294-4
Linear Mold Shrinkage, Transverse 0.0061 cm/cmISO 2577, 294-4
Melt Flow 43.5 g/10 min
@Load 10.0 kg,
Temperature 360 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 205 MPa
@Load 98.0 kg,
Time 30.0 sec
ISO 2039-1
Tensile Strength at Break 125 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 7300 MPaISO 527-1/-2
Izod Impact, Notched (ISO) 6.50 kJ/m²ISO 180/A
Charpy Impact Unnotched 47.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 6.50 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 75-1/-2
 23.0 µm/m-°C
@Temperature 180 °C
DIN 53752
Deflection Temperature at 1.8 MPa (264 psi) 220 °CISO 75-1/-2
Glass Transition Temp, Tg 225 °CISO 11357-1/-2
Decomposition Temperature >= 400 °C
Flammability, UL94 V-0
@Thickness 1.60 mm
Ignition Temperature 580 - 600 °CDIN 54836
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper throat
Zone 1 350 °CFeed zone
Zone 2 360 °CCompression
Zone 3 370 °CMetering-zone
Zone 4 370 °CNozzle
Melt Temperature 350 - 390 °CInjection molding/extrusion
 370 °COptimal
Mold Temperature 150 - 190 °CInjection molding
 170 °COptimal
Drying Temperature 140 °C
Dry Time 4 hour
 
Descriptive Properties
Commercial StatusEurope
Primary Processing TechniqueInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultrason® E 1010 PES
BASF Ultrason® E 6020 P PES
BASF Ultrason® S 3010 MR UN PSU
CENTROPLAST CENTRO HPM Polysulfone
BASF Ultrason® S 2010 PSU

PBASG0173 / 131806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.