MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NuSil MED-4065 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: High consistency rubber, or HCR, consists of high molecular weight polymer combined with silica to produce a material that can be molded, extruded, or calendared into a useful end product. An HCR has the consistency of clay and is primarily formulated in a one or two part system (peroxide and platinum catalysts respectively).

Important Properties: Most platinum cure high consistency rubbers are two component systems with an easy-to-work-with 1:1 mix ratio. Features of platinum cure high consistency rubbers include the following:

  • Two part (typically)
  • Heat accelerated
  • No byproducts
  • Post cure optional
  • Low percent shrinkage
Comments: High Tear

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65Typical
 60 - 70Certified
Tensile Strength at Break 4.80 MPaCertified
 7.90 MPaTypical
Tensile Stress at Strain 350 psi
@Strain 200 %
Elongation at Break 700 %Certified
 950 %Typical
Tear Strength 35.0 pliCertified
 44.1 pliTypical
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 116 °C
Working Life 2.50 hour
@Temperature 25.0 °C
 
Descriptive Properties
Mix Ratio1:1
Plasticity130 mils

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED-4020 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use
NuSil MED-4055 Silicone Ultra High Performance High Consistency Elastomer - Restricted Medical Use
NuSil MED-4960 Liquid Silicone Rubber - Restricted Medical Use

PNUSIL409 / 142133

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.