MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 11, Powder
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Powder

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.35 g/cc0.0361 - 0.0488 lb/in³Average value: 1.14 g/cc Grade Count:79
Water Absorption 1.00 - 2.00 %1.00 - 2.00 %Average value: 1.07 % Grade Count:54
Particle Size 30.0 - 250 µm30.0 - 250 µmAverage value: 82.7 µm Grade Count:58
Thickness 80.0 - 300 microns3.15 - 11.8 milAverage value: 207 microns Grade Count:43
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70.0 - 77.070.0 - 77.0Average value: 71.8 Grade Count:41
Taber Abrasion, mg/1000 Cycles 5.00 - 40.05.00 - 40.0Average value: 17.4 Grade Count:77
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+14 - 2.40e+14 ohm1.00e+14 - 2.40e+14 ohmAverage value: 2.05e+14 ohm Grade Count:5
Dielectric Constant 3.703.70Average value: 3.70 Grade Count:3
Dielectric Strength 7.90 - 66.9 kV/mm201 - 1700 kV/inAverage value: 28.7 kV/mm Grade Count:76
Dissipation Factor 0.01000.0100Average value: 0.0100 Grade Count:3
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 - 193 °C284 - 379 °FAverage value: 185 °C Grade Count:79
Vicat Softening Point 160 - 181 °C320 - 358 °FAverage value: 180 °C Grade Count:41
Flammability, UL94 HB - V-0HB - V-0Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
Overview of materials for Nylon 12, 20% Glass Fiber Filled
Overview of materials for Nylon 12, Carbon Fiber Filled
Overview of materials for Nylon 11 with 10% Glass Fiber Filler

O2635 / 78062

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.