MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese FORTRON 6150T6 PPS, 50% Specialty
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

Material Notes: Fortron 6150T6 is a 50% glass-fiber reinforced and mineral-filled grade with improved impact and heat shock resistance.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0050 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPa5mm/min; ISO 527-2/1A
Elongation at Break 1.6 %5mm/min; ISO 527-2/1A
Tensile Modulus 13000 MPa50mm/min; ISO 527-2/1A
Flexural Strength 200 MPaISO 178
Flexural Modulus 12300 MPaISO 178
Charpy Impact Unnotched 40.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 43.0 µm/m-°CISO 11359-2
Melting Point 280 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 160 °Ccavity
 330 - 340 °Chot runner
Feed Temperature 60.0 - 80.0 °C
Zone 1 290 - 300 °C
Zone 2 310 - 320 °C
Zone 3 330 - 340 °C
Zone 4 330 - 340 °C
Die Temperature 310 - 330 °C
Melt Temperature 310 - 340 °CISO 294
 330 - 340 °C
Mold Temperature 135 - 160 °CISO 294
Drying Temperature 130 - 140 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
Injection Pressure 50.0 - 100 MPa
Hold Pressure 30.0 - 70.0 MPa
Back Pressure <= 3.00 MPa
Screw Speed 50 rpm
@Diameter 55.0 mm
 75 rpm
@Diameter 40.0 mm
 120 rpm
@Diameter 25.0 mm
 
Descriptive Properties
Injection moldingYes
Injection speedfast
Sheet extrusionNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Celanese FORTRON 1342L4 PPS, 40% Specialty
Celanese FORTRON 317 PPS, Unfilled
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced

PHCQ281 / 178736

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.