MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Liveo™ Antifoam M Compound
Categories: Polymer; Thermoset; Silicone

Material Notes: Low-volatile silicone antifoam for use in medical and pharmaceutical applications requiring foam suppression or inhibition.

Information provided by DuPont. This was previously a Dow Corning product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³for silicone fluid only; ISO 1183
Viscosity 3100 cP3100 cPfor silicone fluid only
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.840.84PhEur 1470
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4041.404for silicone fluid only
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact per FDA 21 CFR
 
Component Elements PropertiesMetricEnglishComments
SiO2 4.0 - 7.0 %4.0 - 7.0 %PhEur 1470
 
Descriptive Properties
Aromatic content0.2 ABSPhEur 1470
BasisPDMS + SiO2
ColorGray
Defoaming performance< 15 s20 PPM; PhEur 1470
Heavy metals content< 5 ppm
Polymer((Si)+Compound)
Volatility (%)< 14h at 200°C; PhEur 1470

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4715 / 256164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.