MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AlphaGary PVC FMPP - Clear, Various Colors Polyvinyl Chloride Thermoplastic
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded; PVC, Wire and Cable Grade

Material Notes: Resistant to UV, moisture and mildew for high speed extrusion of coated yarn for outdoors furniture, wire fence coating and automotive harness cable coating

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83
Tensile Strength 2600 psi
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -27.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Molded
AlphaGary PVC FM1R Polyvinyl Chloride Thermoplastic
AlphaGary PVC GEX 03-033 F Natural Polyvinyl Chloride Thermoplastic
Overview of materials for PVC, Extruded
AlphaGary PVC 2212-100 CLEAR 0003 Polyvinyl Chloride Thermoplastic

PGARY9936 / 140722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.