MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Go Yen Chemical Melamine Polyphosphate (MPP) Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 20208-95-1

Applications:

  • Thermal Plastic: TPU, PP, Nylon, PET and related engineering plastic, PE (HDPE, LDPE), POLYOLIFIN, NYLON, POM, ….etc.
  • PC board and other equipments.
  • In various kinds of flame retardant adhesives
  • Thermal Setting: Phenol, Epoxy, Unsaturated Polyester, Polyester Resin, Acrylic Resin …etc.
  • Coatings and Various Resins: Flame Retardant paints, all kinds of Acryl related products, PU, PMMA, Latex, Adhesives
  • Foam Polymers: Applied in multi-kinds of foam Products, especially rigid PU Foam Polymers ,EVA foam materials.
  • Electrical & electronic: connector, switches, housings.
  • Plastic industry : EPDM, CR, NBR, SBR, SIR, CSM, NR. IIR, various kinds of flame retardant, rubber.
  • Elastomer: TPE, TPU, SBS, SEBS, TPR, TPV, various kinds of elastomer.
  • Others: Printing Ink, Pigment, printing, backing glue, flame retardant master batch, plastic panel, paper, furniture plywood, various kinds of flame retardant for electronic products, flame retardant inflatable paint.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 325 Mesh325 Mesh0.001
pH 5.0 - 7.05.0 - 7.0
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 38.3 %38.3 %
Phosphorus, P 32 %32 %
 
Descriptive Properties
AppearanceWhite powder
Solubility0.004g/100ml

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN074 / 266382

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.