MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Gromax PET 9030-104E 30% Glass/Mineral Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Material Notes: Product Description: PET glass 30% reinforced injection molding grade.

Characteristics:

  • Excellent electrical property
  • Excellent mechanic and chemical property
  • Excellent weatherability
  • Excellent wear property
  • Excellent moldability
  • High resistance to fuels, oil, fats and many solvents
  • Low warp age

    Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.54 g/cc1.54 g/ccASTM D792
Moisture Absorption 0.0500 %
@Time 86400 sec
0.0500 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage  0.0010 - 0.0030 cm/cm
@Thickness 1.60 mm
0.0010 - 0.0030 in/in
@Thickness 0.0630 in
horizontal; ASTM D955
 0.0040 - 0.011 cm/cm
@Thickness 1.60 mm
0.0040 - 0.011 in/in
@Thickness 0.0630 in
vertical; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 113 MPa16400 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 170 MPa24700 psiASTM D790
Flexural Modulus 6.86 GPa996 ksiASTM D790
Izod Impact, Notched >= 0.785 J/cm
@Thickness 6.35 mm
>= 1.47 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohm1.00e+13 ohmASTM D257
Dielectric Constant 3.5
@Frequency 60 Hz
3.5
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 2.00 mm
508 kV/in
@Thickness 0.0787 in
ASTM D149
Dissipation Factor 0.0050
@Frequency 60 Hz
0.0050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 257 °C495 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FASTM D648
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 265 - 300 °C509 - 572 °F
Nozzle Temperature 270 - 300 °C518 - 572 °F
Mold Temperature 80.0 - 120 °C176 - 248 °Fsuitable temperature 90-120°C
Injection Pressure 50.0 - 120 MPa7250 - 17400 psi
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 0.000 - 0.300 MPa0.000 - 43.5 psi
Screw Speed 60 - 120 rpm60 - 120 rpmto be chosen in such a way that plasticizing time is just within cooling time
 
Descriptive Properties
Injection Ratemiddle-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fibre Glast 573 Style 120 E-Glass Fiberglass Fabric
Zhejiang Juner PC/PET Alloy
Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant
Kingfa PET-G30 30% Glass Fiber Reinforced PET
E-Polymers Tekaster® F615G30 , 30% Glass Fiber Reinforced PET

PGROM045 / 147858

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.