MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical TR552F MABS, Extrusion, Injection Molding
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Transparency, Softness, No Stress Whitening

Applications: The Edge of Furniture

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82ASTM D785
Tensile Strength, Yield 408 kg(f)/cm²
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Break >= 15 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Tensile Modulus 1450 MPa
@Thickness 3.20 mm
50 mm/min; ASTM D638
Flexural Strength 61.0 MPa
@Thickness 3.20 mm
15 mm/min; ASTM D790
Flexural Modulus 17300 kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Izod Impact, Notched 2.04 kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
 2.04 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 5.10 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 5.10 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
@Thickness 6.40 mm
Unannealed, Edgewise; ASTM D648
Vicat Softening Point 87.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical 50.0 °CUL 746B
UL RTI, Mechanical with Impact 50.0 °CUL 746B
UL RTI, Mechanical without Impact 50.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ASTM D1003
Transmission, Visible 91 %
@Thickness 3.20 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 - 230 °C
Middle Barrel Temperature 220 - 240 °C
Front Barrel Temperature 220 - 240 °C
Nozzle Temperature 220 - 240 °C
Melt Temperature 220 - 240 °C
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 - 90.0 °C
@Time 7200 - 14400 sec
Moisture Content >= 0.010 %
Back Pressure 2.94 - 5.88 MPa
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9957 / 239473

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.