MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior ForTii® MX2 PPA-GF40 PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® MX2 is a high Tg PPA that outperforms in dimensional stability at elevated temperatures due to the high heat deflection temperature (HDT). MX2 has excellent fatigue performance and good chemical resistance. Features: Heat stabilized. 40% glass reinforced. Processing: injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccDry; ISO 1183
Moisture Absorption 1.80 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0035 cm/cmDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cmDry; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 78.0 MPa
@Temperature 200 °C
ISO 527-1/-2
 85.0 MPa
@Temperature 180 °C
ISO 527-1/-2
 90.0 MPa
@Temperature 120 °C
Cond; ISO 527-1/-2
 95.0 MPa
@Temperature 160 °C
ISO 527-1/-2
 100 MPa
@Temperature 100 °C
Cond; ISO 527-1/-2
 105 MPa
@Temperature 150 °C
ISO 527-1/-2
 115 MPa
@Temperature 80.0 °C
Cond; ISO 527-1/-2
 140 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 170 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 190 MPa
@Temperature 40.0 °C
Cond; ISO 527-1/-2
 200 MPa
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 210 MPa
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 220 MPa
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 230 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 250 MPa
@Temperature -40.0 °C
Dry; ISO 527-1/-2
 250 MPa
@Temperature -40.0 °C
Cond; ISO 527-1/-2
Elongation at Break 2.1 %
@Temperature -40.0 °C
Cond; ISO 527-1/-2
 2.1 %
@Temperature 40.0 °C
Cond; ISO 527-1/-2
 2.2 %
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 2.2 %
@Temperature -40.0 °C
Dry; ISO 527-1/-2
 2.2 %
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 2.3 %
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 2.5 %
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 3.0 %
@Temperature 100 °C
Dry; ISO 527-1/-2
 4.5 %
@Temperature 80.0 °C
Cond; ISO 527-1/-2
 5.0 %
@Temperature 100 °C
Cond; ISO 527-1/-2
 5.1 %
@Temperature 120 °C
Dry; ISO 527-1/-2
 6.0 %
@Temperature 120 °C
Cond; ISO 527-1/-2
 6.9 %
@Temperature 150 °C
ISO 527-1/-2
 7.0 %
@Temperature 160 °C
ISO 527-1/-2
 7.0 %
@Temperature 180 °C
ISO 527-1/-2
 7.0 %
@Temperature 200 °C
ISO 527-1/-2
Tensile Modulus 5300 MPa
@Temperature 200 °C
ISO 527-1/-2
 5500 MPa
@Temperature 180 °C
ISO 527-1/-2
 6300 MPa
@Temperature 120 °C
Cond; ISO 527-1/-2
 6300 MPa
@Temperature 160 °C
ISO 527-1/-2
 6700 MPa
@Temperature 150 °C
ISO 527-1/-2
 7000 MPa
@Temperature 100 °C
Cond; ISO 527-1/-2
 8800 MPa
@Temperature 80.0 °C
Cond; ISO 527-1/-2
 9500 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 12800 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 13500 MPa
@Temperature 80.0 °C
Dry; ISO 527-1/-2
 14000 MPa
@Temperature 40.0 °C
Cond; ISO 527-1/-2
 14200 MPa
@Temperature 40.0 °C
Dry; ISO 527-1/-2
 14500 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 14800 MPa
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 14800 MPa
@Temperature -40.0 °C
Dry; ISO 527-1/-2
 15000 MPa
@Temperature -40.0 °C
Cond; ISO 527-1/-2
Flexural Strength 290 MPaCond; ISO 178
 350 MPaDry; ISO 178
Flexural Modulus 5000 MPa
@Temperature 200 °C
ISO 178
 5400 MPa
@Temperature 180 °C
ISO 178
 6000 MPa
@Temperature 160 °C
ISO 178
 9800 MPa
@Temperature 120 °C
ISO 178
 14000 MPa
@Temperature 23.0 °C
Dry; ISO 178
 14500 MPa
@Temperature 23.0 °C
Cond; ISO 178
Fatigue Strength 100 MPa
@# of Cycles 316 ,
Temperature 140 °C
R=0.1, 8 Hz, dry
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature -30.0 °C
Cond; ISO 179/1eU
 60.0 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eU
 65.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
Cond; ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmDry; IEC 62631-3-1
 >= 1.00e+13 ohm-cmCond; IEC 62631-3-1
Dielectric Constant 4.6
@Frequency 1e+6 Hz
Dry; IEC 62631-2-1
 4.8
@Frequency 1e+6 Hz
Cond; IEC 62631-2-1
 4.9
@Frequency 100 Hz
Dry; IEC 62631-2-1
 5.7
@Frequency 100 Hz
Cond; IEC 62631-2-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°CASTM D696
CTE, linear, Parallel to Flow 30.0 µm/m-°CDry; ASTM D696
Melting Point 325 °C10°C/min. Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 175 °CThermal Index; 5000 hrs.; IEC 60216/ISO 527-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 305 °CDry; ISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7911 / 291347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.