MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This flame retardant material, U.L. 94 V0 rated at 0.8 mm, shows high Glow-wire, CTI values and good mechanical properties .It can be supplied in various colors. This grade is suitable for molding insulating parts for electrical devices: switches, rotary switches, timers and contactors. This product is available in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPaISO 527 Type 1A
Elongation at Break 2.5 %ISO 527 Type 1A
Tensile Modulus 8800 MPaISO 527 Type 1A
Izod Impact, Notched (ISO) 9.80 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 500 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 220 °CISO 75/Af
Flammability, UL94 V-0
@Thickness 0.800 mm
1210
 V-0
@Thickness 1.60 mm
1210
 V-0
@Thickness 3.20 mm
1210
Glow Wire Ignition Temperature 775 °C
@Thickness 0.800 mm
ISO 60695-2-13
 775 °C
@Thickness 1.60 mm
ISO 60695-2-13
Glow Wire Flammability Index 960 °CISO 60695-2-12
 960 °CISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 275 - 280 °C
Front Barrel Temperature 280 - 290 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone280-285°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber High Temperature Boards M Ceramic Fiber
Domo TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 V40 Black 21 N PA 66 40% Glass Reinforced, Conditioned
Domo TECHNYL® A 218G2 V50 Black 34N PA 66 50% Glass Reinforced, Conditioned
Domo TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned

PRHOD704 / 137935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.