MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GS Caltex HI-PRENE M540SB PP, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product features: Excellent impact resistance

Final product: Home appliance components (washer, refrigerator, etc.), battery case, automotive components (interior, exterior), industrial components (pallet, crate, etc.)

Information provided by GS Caltex Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow  9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
 9090ISO 2039
Tensile Strength 27.0 MPa3920 psiISO 527
 28.0 MPa4060 psiASTM D638
Elongation at Break >= 250 %>= 250 %ASTM D638
 >= 250 %>= 250 %ISO 527
Flexural Modulus 1.25 GPa181 ksiISO 178
 1.30 GPa189 ksiASTM D790
Izod Impact, Notched  0.350 J/cm
@Temperature -10.0 °C
0.656 ft-lb/in
@Temperature 14.0 °F
ASTM D256
 0.800 J/cm
@Temperature 23.0 °C
1.50 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Temperature -10.0 °C
1.43 ft-lb/in²
@Temperature 14.0 °F
ISO 180
 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FISO 75
 100 °C212 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGSCAL006 / 294880

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.