Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile, impact and puncture strength. The superior strength properties along with excellent draw ability allow down gauging in bag applications. Applications: Trash bags, liners and general packaging. Advantages: Superior strength and excellent draw ability. Information provided by Titan Chemicals |