MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 868-6N3 Room Temperature Cure Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 868-6N3 room temperature cure epoxy is a thixotropic version of TRA-BOND 868-6N1 adhesive. This adhesive provides strong bonds to difficult-to-bond metals, such as gold, silver, copper, brass and solder.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 61000 cP61000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Adhesive Bond Strength 31.7 MPa4600 psiLap shear, alum to alum
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 115 °C239 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 75.0 °C
0.250 hour
@Temperature 167 °F
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
Working Life 15.0 min
@Temperature 25.0 °C
15.0 min
@Temperature 77.0 °F
Shelf Life 3.00 Month
@Temperature -40.0 °C
3.00 Month
@Temperature -40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC178 / 71106

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.