Notes: Medalist MD-50200 Series is a high performance thermoplastic elastomer series, designed to be a sustainable alternative to flexible PVC for medical tubing and film. Medalist MD-50288 is a medium hardness, low density, clear grade, available in NAT and color-matched, intended for use in medical and healthcare applications, with excellent processability and throughput in extruded tubing. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Processing Stability; Halogen Free; High Clarity; High Hardness; High Purity; Kink Resistant; Low Density; Low Specific Gravity; No Animal Derived Components; Radiation (Gamma) Resistant Uses: Clear Sheet; Film; Hose; Medical/Healthcare Applications; Pharmaceuticals; Tubing Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion; Cast Film Information provided by Teknor Apex |