MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Trigonox 101-E32 2,5-Dimethyl-2,5-di(tert-butylperoxy)hexane, 32% solution in mineral oil
Categories: Other Engineering Material

Material Notes: Initiator for the production of controlled rheology polypropylene (CR-PP).

CAS number: 78-63-7

EINECS/ELINCS No: 201-128-1

Applications: Controlled rheology polypropylene: Trigonox 101-E32 is an efficient peroxide for the degradation of polypropylene (CRPP) in the temperature range of 200-250°C. The diluted form of Trigonox 101-E32 in mineral oil allows a more accurate dosage of the peroxide to the polymer. Also a more homogeneous distribution of the peroxide throughout the polymer is of advantage. The white oil acts in PP also as a plasticizer to facilitate molding, e.g. for the fabrication of syringes for injectors.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.865 g/cc
Half-life 0.100
@Temperature 156 °C
[hr]
 1.00
@Temperature 134 °C
[hr]
 10.0
@Temperature 115 °C
[hr]
Viscosity 6.4 cP
Molecular Weight 290.4 g/mol
Storage Temperature <= 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 70.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay31-33 %
Color50 Pt-Co / APHA max.
Content (%)11.02Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY978 / 286501

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.