MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: This mLLDPE is tailored for applications that require:
  • Excellent clarity
  • Excellent gloss
  • Excellent toughness
  • Excellent heat seal

Typical blown film applications include:

  • Seal layer in coextrusions
  • Heavy duty packaging
  • Clarity packaging

This grade contains a process aid and does not contain antiblock or slip agent.

Formerly branded with the MarFlex® trade name. Information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.914 g/ccASTM D1505
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.0 MPaASTM D882
Film Tensile Strength at Yield, TD 9.00 MPaASTM D882
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
Puncture Energy 10.5 JASTM D3763
Coefficient of Friction >= 1.0ASTM D1894
Elmendorf Tear Strength, MD 270 g/milASTM D1922
Elmendorf Tear Strength, TD 360 g/milASTM D1922
Dart Drop 1500 g/milASTM D1709
Film Tensile Strength at Break, MD 61.0 MPaASTM D882
Film Tensile Strength at Break, TD 50.0 MPaASTM D882
1% Secant Modulus, MD 146 MPaASTM D882
1% Secant Modulus, TD 165 MPaASTM D882
Heat Seal Strength Initiation Temperature 95.0 °CASTM F882
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %ASTM D1003
Gloss 135 %at 60°; ASTM D2457
 
Descriptive Properties
Film Puncture Force129 NASTM D3763
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
Chevron Phillips Marlex® D139DK Metallocene Linear Low Density Polyethylene, Blown Film
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin
Chevron Phillips Marlex® D143 m-LLDPE Linear Low Density Polyethylene

PCHEVC922 / 130405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.