MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dynasol Calprene® 484 Thermoplastic Rubber SBS Oil extended
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Calprene 484 is a 56/44 Butadiene/Styrene thermoplastic copolymer, polymerized in solution. It has a radial structure and is extended with 46 phr of paraffinic oil.

This product is presented in pellet form and has very adequate flow properties for compounding articles intended for injection.

Applications:

  • Footwear
  • Sportswear
  • Mechanical rubber goods

Information provided by Dynasol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.40 %<= 0.40 %ASTM D-5668
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
7.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D-1238
Ash <= 0.35 %<= 0.35 %ASTM D-5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 44 %44 %on polymer; ASTM D-5775
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373ASTM D-2240
Abrasion 130130mm³; DIN 53516
 
Descriptive Properties
Hunterlab color, max2
Insolubles in toluene, 325 mesh, % max0.1
Oil Content, %31.5ASTM D-5774

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dynasol Calprene® 485 Thermoplastic Rubber SBS Oil extended
Overview of materials for Styrene/Butadiene/Styrene (SBS)
RTP Company RTP 2740U-80A  Saturated Styrenic Elastomer (SBS) 80 Shore A
Dow AFFINITY™ KC 8852 Polyolefin Elastomer
Dow Engage® 8842 Polyolefin Elastomer

PDYNA40 / 34786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.