Notes: Monprene CP-28114 is a high performance thermoplastic elastomer, available in natural and colors, designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-28114 is a low hardness, low density, lubricated grade that is suitable for injection molding or extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Good Compression Set; Good Flow; Good Melt Strength; Good Mold Release; Good Moldability; Low Compression Set; Low Density; Low Hardness; Low Specific Gravity; Lubricated; Medium Flow; Soft; Without Fillers Uses: Consumer Applications; Gaskets; Handles; Knobs; Rubber Replacement; Tubing RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |