MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BNZ Materials Blakbond Mortar
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Blakbond is a highly refractory mortar which possesses high water retention properties. It is especially designed for laying insulating fire brick and is also used for super duty and high alumina dense refractory brick. It is dark gray in color. Temperature to 3000°F. It is furnished in a consistency suitable for shallow patching or troweling. For a dipping consistency, add approximately 5 qts. of water to 100 lbs. of the as-received Blakbond. Blakbond is a good choice for a single mortar on jobs involving a majority of insulating fire brick and a few dense fire brick.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 123 lb/ft³Dipping, 7% H2O
 131 lb/ft³As received
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00396 GPaDipped Joint; ASTM C198
 0.0421 GPaMortar
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 3000 °F
Shrinkage 4.1 %Permanent Linear Change at Use Limit
 
Component Elements PropertiesOriginal ValueComments
Al2O3 43.1 %
CaO 0.30 %
Fe2O3 1.6 %
K2O 0.90 %
Loss on Ignition(%) 1.7 %
Na2O 2.7 %
SiO2 48.1 %
TiO2 1.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chosun Refractories ZM-2 Special Mortar
Chosun Refractories SM-1 Special Mortar
Chosun Refractories MSM-36 High-Adhesion Mortar
BNZ Materials Super Blakbond Mortar
BNZ Materials No. 2986 Mortar

CBNZ957 / 149197

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.