Vydyne 21LS is a low-viscosity, general purpose PA66 resin used for extrusion-compounding. Vydyne 21LS enables good blending with shear sensitive materials and high-percent filler concentration where distributive mixing is essential to the final product performance. The compounded product will maintain its high flow and performance needed for the application. Vydyne 21LS offers resistance to heat, oil, and wear in line with PA66 neat resins.Information provided by Ascend Performance Materials. |