Lewatit® MDS 1268 K 310 is a food grade, gel-type, monodisperse, strongly acidic cation exchange resin based on a styrene-divinylbenzene copolymer. Because of its fine grain size, it is especially suitable for chromatographic separation, such as the separation of ions from molasses. When using Lewatit MDS 1268 K 310 for the treatment of drinking water and the aqueous solutions mentioned above, the start up recommendations are to be observed, which are available on demand.Information provided by Lanxess. |