Description: Hifax™ HSBMG265 medium high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of rigidity, low temperature impact resistance, dimensional stability and processability. It was designed for use in thin-walled bumper fascia applications that require high paint durability. Uses: Automotive exterior parts Information provided by Basell. |