MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Nanoblend™ LST 5501 Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demanding structural and durability requirements. At the same time, they offer the light weight, aesthetic and processing advantages that are more typical of polyolefins.

Provisional Product Information - Physical and Mechanical properties based on initial production.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.948 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 39.4 MPaType I, 51 mm/min; ASTM D638
Elongation at Yield 5.5 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 3360 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 63.6 MPaASTM D790
Flexural Modulus 2690 MPaASTM D790
Izod Impact, Notched 27.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 45.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Descriptive Properties
Filler / ReinforcementClay Nano Filler
FormsPellets
Generic MaterialPP, Unspecified
Generic NamePolypropylene, Unspecified (PP, Unspecified)
Regional AvailabilityNorth America
 South America

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer)
A. Schulman Diamond NPP30-2000HC Homopolymer Polypropylene
Avient Maxxam™ DP 4980-1-1000 Polypropylene Homopolymer (PP Homopolymer)
Dow 118.01 Performance Polypropylene Polymer
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow, Nucleated, Anti-stat

PH0POL0704 / 145273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.