MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aclo Accucomp ABS ABS892BL High Heat Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0060 cm/cmMD; ASTM D955
Melt Flow 0.80 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength at Break 5510 psiASTM D638
Tensile Strength, Yield 7540 psiASTM D638
Elongation at Break 20 %ASTM D638
Elongation at Yield 4.0 %ASTM D638
Tensile Modulus 246500 psiASTM D638
Flexural Strength 10440 psiASTM D790
Flexural Modulus 377000 psiASTM D790
Izod Impact, Notched 6.90 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 208 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °F
Flammability, UL94 HB
@Thickness 1.59 mm
UL File #E56070

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Stylac™ 20 ABS Polymer
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Aclo Accucomp ABS ABS802L High Impact Grade
Aclo Accucomp ABS ABS801L Medium Impact Grade
Bamberger Polymers Bapolene® 1072 Polyethylene, Injection Grade

PACLO012 / 22267

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.