MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE

Material Notes: Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability, oil, fuel and solvent resistance. It is supplied uncolored in pellet form.

Availability: North America

Additive: Flame Retardant

Features: Flame Retardant, Good Toughness, Oil resistant, Fuel Resistant, Halogen Free, Solvent Resistant, Good Abrasion Resistance and Hydrolytically Stable

Appearance: Colorless

Forms: Pellets

Processing Method: Injection Molding and Extrusion

Information provided by Alliance Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87ASTM D2240
Tensile Strength at Break 3630 psiASTM D412
Tensile Stress at Strain 725 psi
@Strain 100 %
ASTM D412
 1020 psi
@Strain 300 %
ASTM D412
Elongation at Break 600 %ASTM D412
Tear Strength 514 pliDie C; ASTM D412
Taber Abrasion, mg/1000 Cycles 40ASTM D1044
Abrasion 20mm3; DIN 53516
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D3995B
 41 %
@Temperature 70.0 °C,
Time 259000 sec
ASTM D3995B
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 257 °FASTM D1525
Brittleness Temperature -34.6 °FASTM D746
Flammability, UL94 HB
@Thickness 1.00 mm
 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 °CGate Temperature; Extrusion
 401 - 419 °FInjection
Rear Barrel Temperature 365 °FInjection
Middle Barrel Temperature 392 °FInjection
Front Barrel Temperature 401 °FInjection
Nozzle Temperature 401 - 419 °FInjection
Zone 1 365 °FExtrusion
Zone 2 392 °FExtrusion
Zone 3 401 °FExtrusion
Die Temperature 414 °FExtrusion
Mold Temperature 77.0 - 140 °FInjection
Injection Velocity >= 10.0 mm/secInjection
Drying Temperature 185 °FInjection
 185 °FExtrusion
Dry Time 4.00 hourInjection
 4.00 hourExtrusion
Back Pressure 72.5 - 145 psiInjection
Clamp Pressure 5800 - 10200 psiInjection
Screw Speed 60 - 200 rpmInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer
Polymax® Maxelast® D6990 TPE, Extrusion Applications

PAPS084 / 159457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.