MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Parker Chomerics CHO-BOND® 1016 Electrically Conductive Sealant
Categories: Other Engineering Material; Polymer; Thermoset; Silicone

Material Notes: Description: CHO-BOND 1016 sealant is an electrically conductive, one-component RTV silicone which provides both environmental sealing and EMI shielding. This seal, filled with nickel-plated graphite particles, contains no acetic acid, and cures in the presence of moisture at room temperature. Skin formation takes only a few minutes and full property development takes one week. CHO-BOND 1016 sealant is ideal for outdoor enclosure applications where both EMI shielding and galvanic corrosion are requirements. This product should be stored at or below 77°F (25°C)

Features: Excellent resistance to galvanic corrosion, Non-corrosive sealant, Cures in the presence of moisture, Needs no pressure during cure (excellent as a fillet seal), Rapid skin formation.

Application: If CHO-BOND 1016 sealant is being applied to a non-silicone surface, a very thin coating of CHO-BOND 1086 primer must first be applied with a clean cloth. Before applying CHO-BOND 1016 sealant, primer must be allowed to dry 15-30 minutes. (Note: Primer is included in CHO-BOND 1016 sealant package).

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.95 - 2.45 g/cc1.95 - 2.45 g/ccASTM D792
Thickness 180 - 1020 microns7.09 - 40.2 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Shear Strength >= 1.04 MPa>= 151 psiLap; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.95 ohm-cm<= 0.95 ohm-cmDC; ASTM D2739
Shielding Effectiveness <= 50 dB<= 50 dBCH-TP08
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -45.0 °C-49.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 25.0 °C
168 hour
@Temperature 77.0 °F
Shelf Life 9.00 Month9.00 Month
 
Descriptive Properties
BinderSilicone
ConsistencyMedium Paste
Corrosion Resistance15 mgweight loss, CHO-TM 100
Coverage18.1 cm2/g0.0254mm thickness
FillerNickel-plated graphite (Ni/c)
Mix Ratio1-partby weight
Work Life0.5 hr.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME203 / 130913

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.