MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electronic, appliance, automotive and optical industries.

Characteristics:

  • Medium viscosity
  • 20% glass fiber

Applications:

  • 3025R type reinforced by glass fiber (short fiber). particularly suitable for injection molding where especially good dimensional stability is required

All information provided by Samyang

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Water Absorption 0.12 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Thickness 3.00 mm
ASTM D955
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ASTM D785
Tensile Strength, Yield 1100 kg(f)/cm²ASTM D638
Elongation at Break 9.0 %ASTM D638
Flexural Yield Strength 1700 kg(f)/cm²ASTM D790
Flexural Modulus 50000 kg(f)/cm²ASTM D790
Izod Impact, Unnotched 16.0 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+16 ohm-cmASTM D257
Dielectric Constant 3.11
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 31.0 kV/mmASTM D149
Dissipation Factor 0.0097
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.0 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 151 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 147 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 300 °C
Middle Barrel Temperature 280 - 300 °C
Front Barrel Temperature 280 - 300 °C
Nozzle Temperature 290 - 310 °C
Melt Temperature 300 - 310 °C
Drying Temperature 120 °C
Dry Time 3 - 5 hour
Moisture Content <= 0.020 %
Screw Speed 30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® DP1-1888 Polycarbonate, 20% Glass Filled
Lotte Advanced Materials Starex® HG-0760GP ABS
Asahi Kasei Thermylene® P4-30FG-0522 PP-GF30FR
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry)
Ascend Performance Materials Vydyne® R413H BK07 Impact Modified Nylon 66, 13% Glass Filled

PSAMY082 / 88164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.