MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Tailoring NK Intumescent System
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: NK is our second fully formulated single shot intumescent system, specifically suited to low temperature processing applications. We are working towards achieving REACH registration for NK in 2018.
  • High phosphorus content
  • Single component intumescent system
  • Limited water solubility
  • Good thermal stability
  • Small particle size
  • Neutral pH in aqueous systems
Typical Applications: NK is the ideal choice whenever a high degree of flame retardancy is desired, without the use of halogen, in paints, coatings, sealants, mastics and adhesives.

Information provided by Polymer Tailoring Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.630 g/cc0.0228 lb/in³
Density 1.22 g/cc0.0441 lb/in³
Particle Size <= 10 µm<= 10 µm50% median
pH 7.07.010% slurry
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 19.5 %19.5 %
 
Descriptive Properties
AppearanceWhite, free-flowing powder
Component0Halogen
Solubility3 g/100g water
Thermal Stability15% weight loss 300°CThermogravimetric analysis (TGA) at 20°C/min
 2% weight loss 250°CThermogravimetric analysis (TGA) at 20°C/min
 30% weight loss 400°CThermogravimetric analysis (TGA) at 20°C/min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTAIL001 / 297039

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.