MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Magnesium HM31A O Wrought Alloy (UNS M13312)
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Mg-3Th-1.2Mn

Key Words: UNS M13312
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 283 MPa
Tensile Strength, Yield 230 MPa
@Strain 0.2 %
Elongation at Break 10 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.0 µm/m-°C
Specific Heat Capacity 1.05 J/g-°C
Thermal Conductivity 104 W/m-K
Melting Point 605 - 650 °C
Solidus 605 °C
Liquidus 650 °C
 
Component Elements PropertiesOriginal ValueComments
Magnesium, Mg 95.8 %As balance
Manganese, Mn 1.2 %
Thorium, Th 3.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium AM100A-T5, Cast
Parkway Products Thixomolded® AM50A Magnesium
Magnesium Alloys, General
Magnesium AE42-F, Die Cast
Magnesium AM100A-T4, Cast

MMHM31AO / 100317

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.