MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Eastar GN071 Natural PETG Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: Product Description: Eastar™ GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions will not turn Eastar™ GN071 white. This makes this product one of our most versatile materials for the cosmetics and personal care packaging market. Eastar™ GN071 Copolyester is certified to NSF/ANSI Standard 51 for Food Equipment Materials. This product has been GREENGUARD INDOOR AIR QUALITYCERTIFIED

Applications/Uses:

  • Cosmetic jars
  • Cosmetics/personal care packaging
  • Credit cards
  • Debit cards
  • Furniture guards
  • Furniture/Furniture trim
  • Gaming cards
  • Gift cards
  • Housewares
  • Identification cards
  • Phone cards
  • Plastic Cards
  • Smart cards
  • Stationery supplies
  • Toys/Sporting goods
  • Writing instruments
Key Attributes:
  • Easy to extrude, cut, print, and seal
  • Effective barrier properties
  • Excellent chemical resistance
  • Excellent clarity
  • Excellent colorability
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Toughness

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0050 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength at Break 29.0 MPa4210 psiISO 527
 30.0 MPa4350 psiASTM D638
Tensile Strength, Yield 48.0 MPa6960 psiISO 527
 50.0 MPa7250 psiASTM D638
Elongation at Break 180 %180 %ASTM D638
 200 %200 %ISO 527
Elongation at Yield 4.0 %4.0 %ISO 527
 4.4 %4.4 %ASTM D638
Tensile Modulus 2.00 GPa290 ksiISO 527
 2.03 GPa294 ksiASTM D638
Flexural Strength 67.0 MPa9720 psiISO 178
Flexural Yield Strength 68.0 MPa9860 psiASTM D790
Flexural Modulus 2.06 GPa299 ksiASTM D790
 2.10 GPa305 ksiISO 178
Izod Impact, Notched 1.05 J/cm1.97 ft-lb/inASTM D256
 0.400 J/cm
@Temperature -40.0 °C
0.749 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Izod Impact, Notched (ISO)  4.40 kJ/m²
@Temperature -40.0 °C
2.09 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 9.40 kJ/m²
@Temperature 23.0 °C
4.47 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FISO 75 and ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FISO 75 and ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 0.20 %0.20 %ASTM D1003
Transmission, Visible 90 %90 %Total Transmittance; ASTM D 1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °F
Drying Temperature 63.0 °C145 °F
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PETG Copolyester
Eastman Eastar 6763 PETG Copolyester
Eastman PROVISTA Copolymer PETG Copolyester
Eastman Eastar GN007 PETG Copolyester
Changzhou Jinlibao GETAILONG JLB-110900 Clear PETG sheet

PEA045 / 35224

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.