MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo Celanex® 2302 ICF15 PBT/PET, 15% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Mineral Filled; Polyethylene Terephthalate (PET)

Material Notes: Product Description: Chemical abbreviation according to ISO 1043-1: PBT Molding compound ISO 7792-PBT/PET, MGHR, 08-060N, CF15 PBT, polymer blend, 15% carbon fiber reinforced, injection molded parts with superior gloss.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Carbon Fiber

Additive: Mold Release

Features: Antistatic; Good Heat Resistance

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183
Water Absorption 0.15 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.45 %ISO 62
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cmISO 294-4
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 265 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 19600 psiISO 527-2/5
Elongation at Break 3.4 %ISO 527-2/5
Tensile Modulus 1.81e+6 psiISO 527-1
Charpy Impact Unnotched 24.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.80 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 2.40 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 200 ohm-cmIEC 62631-3-1
Surface Resistance 70000 ohmIEC 62631-3-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 78.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 61.0 µin/in-°FISO 11359-2
Melting Point 491 °FISO 11357-3
Deflection Temperature at 8.0 MPa 149 °FUnannealed; ISO 75-2/C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 122 °FHopper
 509 - 527 °FHot Runner
Feed Temperature 374 - 392 °FInjection
Rear Barrel Temperature 482 - 500 °F
Middle Barrel Temperature 482 - 500 °F
Front Barrel Temperature 500 - 518 °F
Nozzle Temperature 509 - 527 °F
Zone 4 500 - 518 °FInjection
Melt Temperature 509 - 527 °F
Mold Temperature 194 - 212 °F
Drying Temperature 248 - 284 °F
Dry Time 2.00 - 4.00 hour
Screw Speed 60 rpm
@Thickness 55.9 mm
 75 rpm
@Thickness 40.6 mm
 90 rpm
@Thickness 24.9 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6179 / 310872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.