Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very good chemical resistance. This lower viscosity is also much easier to machine compared to most other epoxies. It has a 100 to 70 mix ratio by weight and a very convenient one to one ratio by volume. EP33LV cures readily at room temperature or more rapidly at elevated temperatures. To optimize its properties, the recommended cure schedule is overnight at room temperature followed by a post cure at 150-200°F for 2-3 hours. After curing, this system has an exceptionally high temperature resistance, serviceable up to 450°F. It resists a range of chemicals including water, oils, fuels and many acids and bases. EP33LV bonds well to a wide variety of substrates including metal, glass, ceramics and many rubbers and plastics. It is a reasonably good electrical insulator. EP33LV is 100% reactive and does not contain any diluents or solvents. The color of Part A is gray, Part B is amber. It is widely used in aerospace, electronic, electrical and specialty OEM type applications. Product Advantages: - Convenient mixing: one to one ratio by volume.
- Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly.
- High temperature resistance up to 450°F.
- Excellent chemical resistance.
- Outstanding dimensional stability.
- Readily machinable.
- Good adhesion to a wide variety of substrates.
Information provided by MasterBond® |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |