MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reade Advanced Materials Zirconium Silicate (Zircon) Powder (ZrSiO4)
Categories: Ceramic; Oxide; Silicon Oxide; Zirconium Oxide

Material Notes: Description: A fine white mineral powder that is chemically inert and stable to very high temperatures. Insoluble in water, dilute acids and hot concentrate sulfuric acid. Used as a primary source for investment casting shell molds, foundry cores, metal chills, ladle brick, welding rod coatings, abrasive cleaning, and mold washes.
Forms Available: -50+270 mesh, -60+200 mesh, -200 mesh and -325 mesh

Information provided by Reade Advanced Materials.

Key Words: ZrSiO4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.50 - 4.60 g/cc
Bulk Density 2.76 - 2.92 g/cc
Molecular Weight 183.1 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 7.5 - 8.0
 
Thermal PropertiesOriginal ValueComments
Melting Point 2200 - 2550 °C
 
Descriptive Properties
Coloroff white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Anderman Ceramics EZZ 66P Zircon
Zirconium Oxide, Zirconia, ZrO2
Zirconium Orthosilicate, ZrSiO4 (Zircon)
Goodfellow Leachable Ceramic (Silica, Zircon, Alumina)
Accuratus MACOR Machinable Glass Ceramic

CREADE023 / 1956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.