MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch® 226 Solvent Resistant Masking Tape
Categories: Polymer; Adhesive

Material Notes: Scotch® Solvent Resistant Masking Tape 2267 has a film backing that is resistant to many solvent and water based solutions.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.270 milASTM D3652
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22.0 MPaASTM D3759
Elongation at Break 11 %ASTM D3759
Peel Strength 2.625 plito Steel; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 107 °Cup to 30 mins
 
Descriptive Properties
Adhesive TypeRubber
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch® 232 High Performance Masking Tape
3M Scotch® 231A Performance Masking Tape
3M Scotch® 231 Performance Masking Tape
3M Scotch® 222 High-temperature Fine Line Masking Tape
3M Scotch® 22 Heavy Duty Vinyl Electrical Tape

PMM34025 / 168772

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.